Violation Detail
Standard Cited: 19260350 F04 Gas welding and cutting.
Inspection Nr: 1271630.015
Citation: 01004
Citation Type: Serious
Abatement Status: Not Completed - Worksite Changed
Initial Penalty: $4,269.00
Current Penalty: $4,269.00
Issuance Date: 04/17/2018
Nr Instances: 1
Nr Exposed: 4
Abatement Date: 04/27/2018
Gravity: 10
Report ID: 0317000
Contest Date:
Final Order: 05/15/2018
Related Event Code (REC):
Emphasis:
Type | Latest Event | Event Date | Penalty | Abatement Due Date | Citation Type | Failure to Abate Inspection |
---|---|---|---|---|---|---|
Penalty | Z: Issued | 04/17/2018 | $4,269.00 | 04/27/2018 | Serious |
Text For Citation: 01 Item/Group: 004 Hazard:
29 CFR 1926.350(f)(4): Hose which has been subject to flashback, or which shows evidence of severe wear or damage, shall be tested to twice the normal pressure to which it is subject, but in no case less than 300 p.s.i. Defective hose, or hose in doubtful condition, shall not be used: a) Jobsite: Employees conducting iron cutting work used a frayed hose attached to acetylene cylinder during cutting activities. Condition was observed on or about 19 OCT 2017 and 3 NOV 2017.